Progress report to sponsors in the surfacing division, The Welding Institute

Show simple item record

dc.creator Apps, R. L.
dc.date 2016-01-22T12:05:25Z
dc.date 2016-01-22T12:05:25Z
dc.date 19
dc.date.accessioned 2022-05-09T09:55:01Z
dc.date.available 2022-05-09T09:55:01Z
dc.identifier http://dspace.lib.cranfield.ac.uk/handle/1826/9661
dc.identifier.uri https://reports.aerade.cranfield.ac.uk/handle/1826.2/4271
dc.description Since the last report to sponsors circulated in mid-1967, considerable concern has been felt over the wide scatter of results. The scatter in results between specimens produced in a single batch was generally comparatively small, in the order of 15%, but occasional results occurred which ehow6d much greater differences from the average. Identical experiments carried out in different batches exhibited rather more scatter than with in single batches. Similar scatter was noted in the results of other workers" 2 . Additionally, many blasting variables which had previously been considered important by metal sprayers appeared to have very little effect on the bond strength of flame sprayed aluminium coatings on mild steel. Consideration of scatter in results suggested four possible reasons for this scatter.
dc.language en
dc.publisher College of Aeronautics
dc.relation CoA/M-166
dc.relation 166
dc.title Progress report to sponsors in the surfacing division, The Welding Institute
dc.type Report


Files in this item

Files Size Format View
COA_Memo_166.pdf 5.371Mb application/pdf View/Open

This item appears in the following Collection(s)

Show simple item record

Search AERADE


Browse

My Account